產(chǎn)品參數(shù)
le="width: 98%" border="0" cellspacing="1" cellpadding="0">
性能項(xiàng)目 |
試驗(yàn)條件[狀態(tài)] |
測(cè)試方法 |
測(cè)試數(shù)據(jù) |
數(shù)據(jù)單位 |
物理性能 |
熔體流動(dòng)速率 |
220℃×10kg |
ASTM D-1238 |
22 |
g/10min |
熔體流動(dòng)速率 |
200℃×5kg |
ASTM D-1238 |
1.8 |
g/10min |
比重 |
|
ASTM D-792 |
1.05 |
23/23℃ |
機(jī)械性能 |
彎曲強(qiáng)度 |
|
ASTM D-790 |
11200 |
lb/in2 |
彎曲彈性率 |
|
ASTM D-790 |
3.8×105 |
lb/in2 |
引張強(qiáng)度 |
|
ASTM D-638 |
480 |
kg/cm2 |
引張強(qiáng)度 |
|
ASTM D-638 |
6800 |
lb/in2 |
IZOD沖擊強(qiáng)度 |
1/8" |
ASTM D-256 |
3.7 |
ft.lb/in |
彎曲彈性率 |
|
ASTM D-790 |
2.7×104 |
kg/cm2 |
彎曲強(qiáng)度 |
|
ASTM D-790 |
790 |
kg/cm2 |
洛氏硬度 |
|
ASTM D-785 |
116 |
R |
IZOD沖擊強(qiáng)度 |
1/4" |
ASTM D-256 |
18 |
kg.cm/cm |
IZOD沖擊強(qiáng)度 |
1/4" |
ASTM D-256 |
3.3 |
ft.lb/in |
IZOD沖擊強(qiáng)度 |
1/8" |
ASTM D-256 |
20 |
kg.cm/cm |
伸長(zhǎng)率 |
|
ASTM D-638 |
20 |
% |
熱性能 |
熱變形溫度 |
|
ASTM D-648 |
88(190) |
℉ |
維卡軟化點(diǎn) |
|
ASTM D-1525 |
105 |
℃ |
燃燒性 |
File No. E56070 UL&C-UL |
|
1/16"HB |
|
維卡軟化點(diǎn) |
|
ASTM D-1525 |
221 |
℉ |
熱變形溫度 |
|
ASTM D-648 |
99(210) |
℃ |